Hastelloy C22 Round Bars

Pacific Steels & Alloys is manufacturer, supplier, traders and stockiest of highly ranked grades of Hastelloy C22 Round Bars as compared to ordinary dealers. We provide Hastelloy C22 Round Bars in various sizes, shapes, thickness, designs, dimensions and specification of wide range of all sectors. Equivalent Grades of Hastelloy C22 Round Bars is UNS N06022. We also provide extensive collection of products to the Domestic and International clients on demands.

Hastelloy C22 are versatile primary solid solution nickel metallic element Mo metal alloy with increased resistance to roughness, crevice corrosion and stress corrosion cracking. Hastelloy C22 additionally has wonderful resistance to oxidizing binary compound media as well as wet gas and mixtures containing acid or oxidizing acids with gas ions. Hastelloy C22 Round Bar are used for various applications such as Flue gas scrubbers, Chlorination systems, Acid production and Pickling systems, Chemical process, Food processing, Petrochemicals, Pollution control, Pulp and Paper, Refining and Waste treatment facility.

We also supply Hastelloy C22 Square Bar, Duplex steel Hastelloy C22 Hex Bar, Hastelloy C22 Flat Bar, Hastelloy C22 Forged Bar, Hastelloy C22 Bright Bar, Hastelloy C22 Black Bar, Hastelloy C22 Threaded Bar, Hastelloy C22 Polished Bar and Hastelloy C22 Rectangular Bar.

We offer Hastelloy C22 Round Bar at an Economical Price to our customer

For more info feel free to mail us at Sales@psalloys.com

Hastelloy C22 Round Bars Specification

Standard ASTM B574 / ASME SB574
Finish Bright, Polish & Black
Form Round, Square, Hex (A/F), Rectangle, Wire (Coil Form), Wire-mesh, Billet, Ingot, Forging Etc.
Grade Hastelloy C22 (UNS N06022)

Hastelloy C22 Round Bars Chemical Composition

Element Hastelloy C22
Ni Bal
C 0.01 max
Mn 0.50 max
Co 2.5 max
S 0.02 max
Si 0.08 max
Cr 20 – 22.5
Mo 12.5 – 14.5
Fe 2 – 6
W 2.5 – 3.5
v 0.35 max
P 0.02 max

Hastelloy C22 Round Bars Mechanical Properties

Element Hastelloy C22
Density 8.69 g/cm3
Melting Point 1399 °C (2550 °F)
Tensile Strength Psi – 1,00,000 , MPa – 690
Yield Strength (0.2%Offset) Psi – 45000 , MPa – 310
Elongation 45 %
Hardness (Brinell)